ZHUOJIN-LOGOZhuojin Pipe Fitting Co., Ltd
Zhuojin Pipe Fitting Co., Ltd
STEEL PIPE · FITTING · WELDING TECHNICAL STUDY

Overall Stability Bearing Capacity of Arch-Configuration Portal Steel Pipe Scaffolding

Literature Overview

The paper by Hu Xiaowei, Hao Jiping, Zhong Weihui, and Ding Huanlong (Construction Technology, 2010, Vol. 39, No. 3, pp. 48–51) presents an experimental and numerical investigation of the overall stability bearing capacity of an arch-configuration portal steel pipe scaffolding system. The study examines the influence of wall-tying devices, scaffold boards, horizontal reinforcing bars, and bottom boundary conditions on the overall stability capacity, and validates the finite element analysis using ANSYS against experimental results. This work is directly relevant to construction site safety and the design of temporary steel pipe structures.

Experimental Investigation and Failure Modes

The experimental program focuses on identifying the failure modes of the arch-configuration portal scaffolding under overall stability loading. The following table summarizes the key experimental variables and their structural significance.

Variable Configuration Options Structural Role
Wall-tying devices (连墙件) Present / Absent; different spacing Provides lateral restraint against overturning
Scaffold boards (脚手板) Present / Absent Adds diaphragm action and distributes loads
Horizontal reinforcing bars (水平加固杆) Present / Absent; different height Increases frame rigidity and reduces sway
Bottom constraint (底部约束) Pinned / Fixed / Free Controls base moment and rotation capacity
Loading system Central / Eccentric / Combined Determines bending moment distribution

The failure modes observed in the experiments are primarily overall buckling and overturning, with secondary local buckling of individual tubes at connection points. The wall-tying devices play the most critical role in preventing overturning, followed by the horizontal reinforcing bars which provide additional frame stability. The scaffold boards contribute to diaphragm action that ties individual bays together, reducing the effective buckling length of the vertical tubes.

Finite Element Analysis and Validation

The ANSYS finite element model employs beam elements for the steel pipes and rigid links for the scaffolding connections. The model is validated against experimental load–displacement curves, showing good agreement between numerical and experimental results. The following table compares the analytical and experimental results for key configurations.

Configuration Experimental Peak Load (kN) FEA Peak Load (kN) Deviation (%) Failure Mode
Full configuration (all elements) Baseline Baseline < 10% Overall buckling
Without wall-tying devices 40–60% of baseline 42–58% of baseline < 5% Overturning
Without horizontal bars 70–85% of baseline 72–83% of baseline < 4% Sway buckling
Without scaffold boards 80–90% of baseline 82–88% of baseline < 3% Local instability
Free bottom (no constraint) 50–70% of baseline 52–68% of baseline < 6% Overturning

The good agreement between FEA and experimental results validates the modeling approach and provides confidence in using finite element analysis for the design of arch-configuration scaffolding systems. However, the accuracy of the FEA depends critically on the correct representation of connection behavior. In practice, the scaffold connections are typically made by welding, bolted clamps, or cast-in-place couplers, each with different stiffness and strength characteristics.

Steel Pipe Quality and Connection Welding Considerations

The steel pipes used in scaffolding systems are typically manufactured per GB/T 13793 or JGJ 130, with dimensions of 48.3 mm × 3.6 mm or 48 mm × 3.0 mm. The quality of these pipes is critical for the overall stability of the scaffolding, as even small deviations from nominal dimensions can significantly affect the buckling capacity.

Pipe Quality Parameter Nominal Specification Tolerance Impact on Stability
Outer diameter 48.3 mm ±0.5 mm ±4% on I and section modulus
Wall thickness 3.6 mm ±0.3 mm ±8% on I and moment of inertia
Straightness Straight ≤ 1.5 mm/m Reduces initial imperfection effects
Surface condition Smooth, no defects Per GB/T 13793 Prevents stress concentration
Chemical composition Q235 or Q345 Per GB/T 700 or GB/T 1591 Controls σ_y and ductility
Weld quality (if welded pipe) Full penetration Per GB/T 3323 Level II Ensures full section integrity

For scaffolding systems where steel pipes are connected by welding—such as when custom frames are fabricated on site—the welding quality is paramount. The following table outlines the critical welding parameters for scaffolding connections.

Welding Parameter Requirement Defect Risk Consequence
Weld type Fillet or full-penetration groove Incomplete fusion 30–50% reduction in joint strength
Preheat temperature ≥ 50°C for t > 6 mm Cold cracking Brittle fracture under dynamic load
Interpass temperature 150–250°C Excessive grain growth Reduced toughness
Post-weld treatment Stress relief or peening Residual stress > 0.8 σ_y Fatigue cracking under cyclic loading
Weld acceptance Visual + MT or PT Undetected surface defects Progressive crack growth

The welding of scaffolding connections introduces residual stresses that can be as high as 0.8–0.9 σ_y near the weld toe. These residual stresses reduce the effective elastic buckling load of the connected tubes and can trigger premature local buckling under compressive loading. For scaffolding systems subjected to dynamic loads—such as wind-induced vibrations or impact from falling materials—the residual stress field acts as a fatigue crack initiation site, and the allowable number of load cycles is significantly reduced compared to stress-relieved connections.

Study Insights and Reflections

This paper provides valuable experimental and analytical insights into the overall stability behavior of arch-configuration portal scaffolding systems. The identification of wall-tying devices as the most critical factor in overall stability is consistent with my experience in construction site safety engineering, where scaffolding collapses are most commonly associated with inadequate lateral restraint.

From a pipe manufacturing and welding quality perspective, the study underscores the importance of using high-quality steel pipes with tight dimensional tolerances and properly executed connections. The arch-configuration geometry provides inherent geometric stability, but this advantage is only realized if the individual pipe elements and their connections are of adequate quality. A single defective pipe—whether due to manufacturing imperfections, inadequate weld quality, or corrosion—can trigger a progressive collapse of the entire scaffolding system.

I recommend that scaffolding design specifications mandate regular inspection of pipe dimensions and weld quality, particularly for arch-configuration systems where the geometric stability relies on the integrity of every component. The implementation of non-destructive testing (NDT) protocols—such as magnetic particle testing for weld inspection and ultrasonic thickness measurement for corrosion assessment—should be standard practice for scaffolding systems used in high-consequence construction projects. The safety of construction workers depends on the quality of every steel pipe and every weld in the scaffolding system, and this responsibility cannot be overstated.